Syrebestandigt mursten til skorstenis made of pottery clay and clay as the main raw materials, through mixing, molding, firing and other processes to produce acid resistant products. The product has high acid resistance and is not easy to be oxidized under normal temperature. Besides hydrofluoric acid and thermal phosphoric acid, it has excellent anti-corrosion effect on many acid substances. It er vidt brugt i elektrisk strøm, metallurgi og andre skorstene og flues .
1. Funktioner afSyrebestandigt mursten til skorsten:
1) Høj sur modstand, større end eller lig med 97%, god antikorrosionseffekt på de fleste syrerprodukter
2) Ændring af små volumen, god korrosionsbestandighed
3) Farve er lilla rød
2. Anvendelse: skorsten, røggasforing . Derudover bruges det i antikorrosionsudstyr i olie, kemisk industri, kemisk gødning og andre industrier .
The main component of acid resistant brick is SiO2, which forms a lot of polyaluminal Andalusite in the process of high temperature sintering. It is a kind of material with high acid resistance. The acid resistant brick has compact structure (density>=2.4g/cm3), low water absorption, and can withstand any concentration of acid Medium ved stuetemperatur . Produkterne er opdelt i tung mursten og let mursten, som begge har god syremodstandsatmosfære, luft erosion og erosion ydelse . De er vidt brugt i røggas, skorsten, koksovn og kemisk ovn.
3. Produktet er vidt brugt i store skorstene, flues og koksovne i Kina og eksporteret til Sydøstasien og andre lande
4. Vores virksomhed er fri til at give brugerne teknologi, brug og andre tjenester .
Vil du finde en professionel leverandør af ildfaste produkter?
Vil du finde en stabil og troværdig leverandør?
Kontakt derefter med os
Kontakt mig:
E -mail: wp@cnjingganrefractory.com/sdwenping@163.com
Tlf: 86-0533-4188518 / fax: 86-0533-4188518
Rose: +86-13275332819 (WeChat/WhatsApp -nummer)